Message pakhat dah la .

1. Feeder hnathawh chhung hian amplitude, vibration motor current leh motor surface temperature te chu enfiah fo tur a ni. Amplitude chu a hma leh a hnuah a inang vek tur a ni a, a sir leh a sir lamah a inher chhuak tur a ni lo va, vibration motor current pawh a stable tur a ni. Thil awmdan pangngai lo hmuh a nih chuan tihtawp nghal tur a ni.

2. Vibration motor bearing-a lubrication hi feeder pumpui hnathawh dan pangngaia kalpui theihna tur key a ni. Hman chhung hian bearing chu difluidized molybdenum 2# grease hmanga khat reng tur a ni a, thla hnih danah vawi khat, thla tin high temperature season-ah dah tur a ni. Vawikhat chu motor chu thla ruk danah an tichhia a, an siam that a, an chhunga bearings te chu an thlak leh thin.