Burner beam kiln a ni a.

Inquiry thawn rawh .
Burner beam kiln a ni a.
Kimchang
A siam chhuah theihna: 200~800T/D, a tha ber: 500~600T/D
Operating flexibility chu 70%-110% a ni.
Fuels: Gas, solid, liquid .
A lumna a tlem: 820~900kcal/kg. Lime a ni a.
Bithliahna
Lime siam chhuahna line .
Share to
Hrilhfiahna

 

A siam chhuah theih zat: 100~500T/D

Operating flexibility chu 70%-110% a ni.

Fuels: Gas, solid, liquid .

Heat hman tlem: 1000~1200kcal/kg. Lime a ni a.

Exchange exhaust air inthlengna temperature chu 60~100℃aia hniam a ni .

Parallel flow calcination, lime quality chu a inang tlang vek a ni.

LOI 5% aia tlem emaw a tlukpui emaw .

Lime quality: the reactivity >340ml a ni.

product-434-434

product-529-465

 

 

Dingzheng Group hi tuna ram chhunga professional professional ber a ni a, lime kiln industry-ah engineering design, hmanrua siam dan, installation, operation, training, commissioning, leh start{{0}Up te inzawmkhawm a ni. S s a ni.

 